Anóidí íobartacha muirí

Anóidí íobartacha mara: Cosaint riachtanach do do shoitheach

 

Marine sacrificial anodes are protective components made from reactive metals like zinc, aluminum, or magnesium, designed to prevent corrosion on boats and underwater metal structures. By leveraging the principle of galvanic corrosion, these anodes intentionally corrode first, "sacrificing" themselves to divert damage away from critical parts such as hulls, propellers, and RUDDERS . atá riachtanach do thimpeallachtaí sáile agus fionnuisce araon, leathnaíonn siad go mór saolré an trealaimh mhuirí trí é a chosaint ó dhíghrádú leictriceimiceach . Cinntíonn siad go rialta cosaint leanúnach, ag laghdú costais chothabhála agus ag cur cosc ar dhamáiste struchtúrach. ag EHISENENCENCENCENCE ARODANCENCENCE ARODANCENTACE ARODANCENCES. Friotaíocht creimthe is fearr, ag cuidiú le húinéirí soithí a gcuid infheistíochtaí a chosaint i ngach coinníoll uisce .

trawlers-at-the-dry-dock-2025-03-05-03-15-21-utc

 

{1. Anóid íobartach cóimhiotal alúmanaim

 

 

 

20250624172345
 

I measc na n-alúmanam cóimhiotail a úsáidtear go coitianta tá an tsraith al-Zn-in agus an tsraith al-Zn-HG, atá oiriúnach do chosaint chatóide na struchtúr amhail longa in áiseanna uisce mara, calafoirt agus mara, córais fuaraithe uisce farraige, agus an t-uisce taiscthe tancanna stórála {}}} Sraith ALUMOY ALUMOY Andodes comhlíonann an GB {}} a chomhlíonann an GB} an t-al-al-ALU. Anóidí íobartach cóimhiotail . "

 

Bíonn tionchar ag comhdhéanamh ceimiceach an chóimhiotail . ar fheidhmíocht anóid alúmanaim . chun riachtanais na gcustaiméirí a chomhlíonadh agus is féidir linn anóidí a mhonarú le cumadóireachtaí ceimiceacha speisialta bunaithe ar shonraíochtaí custaiméirí .

Iarr luachan

 

 

 

Sonraíochtaí Táirgí

 

 

 

{1. Anóidí íobartacha le haghaidh áiseanna innealtóireachta calafoirt agus innealtóireachta mara .

Múnla

Toisí (a × (b 1+ b2) × c) / mm

Meáchan / kg

Al -1

2300 × (220+240) × 230

310.0

Al -2

1600 × (200+210) × 220

190.0

Al -3

1500 × (170+200) × 180

130.0

Al -4

900 × (150+170) × 160

58.0

Al -5

1500 × (148+178) × 170

120.0

Al -6

850 × (180+220) × 180

85.0

Al -7

800 × (200+280) × 150

80.0

Al -8

700 × (160+220) × 180

72.5

Al -9

1250 × (115+135) × 130

56.0

Al -10

1000 × (115+135) × 130

46.0

Al -11

750 × (115+135) × 130

35.0

Al -12

500 × (115+135) × 130

23.0

freight-port-2025-03-08-17-11-29-utc

I measc na n-alúmanam cóimhiotail a úsáidtear go coitianta tá an tsraith al-Zn-in agus an tsraith al-Zn-HG, atá oiriúnach do chosaint chathóideacha struchtúir amhail:

Longa i sáile

Áiseanna Port agus Mara

Córais Fuarú Sáile

Limistéir uisce taiscthe umar stórála

 

Comhlíonann táirgeadh anóid alúmanaim an caighdeán GB {4948-2002 (anóidí íobartacha al-zn-in-in-in-in-anóidí íobartacha) .

Braitheann feidhmíocht anóid alúmanaim ar a gcomhdhéanamh ceimiceach . Cuirimid foirmlithe cóimhiotail éagsúla ar fáil chun riachtanais na gcustaiméirí a chomhlíonadh agus is féidir leo anóidí a mhonarú le comhdhéanamh ceimiceach saincheaptha ar iarratas .

{2. Anóidí íobartacha le haghaidh taobh istigh umar stórála

Múnla

Toisí (a × (b 1+ b2) × c) / mm

Meáchan / kg

AC -1

750 × (115+135) × 130

35.0

AC -2

500 × (115+135) × 130

23.0

AC -3

500 × (105+135) × 100

16.0

AC -4

300 × (105+135) × 100

10.0

tank

 

 

{3. Anóidí íobartacha le haghaidh umair uisce ballasta

Múnla

Toisí (a × (b 1+ b2) × c) / mm

Meáchan / kg

Ag -1

500 × (115+135) × 130

23.0

Ag -2

1500 × (65+75) × 70

21.5

Ag -3

500 × (110+130) × 120

20.0

Ag -4

1000 × (58.5+78.5) × 68

13.2

Ag -5

800 × (56+74) × 65

10.0

Ag -6

1150 × (48+54) × 51

9.0

Ag -7

250 × (80+100) × 85

5.0

Ag -8

200 × (70+90) × 70

3.0

20250625095830

 

 

{4. Anóidí íobartacha a úsáidtear go coitianta le haghaidh córais fuaraithe uisce farraige

Múnla

Toisí (a × (b 1+ b2) × c) / mm

Cur síos cruth

Meáchan / kg

AE -1

1200 × (200+280) × 150

Traipéisólach

120.0

AE -2

800 × (200+280) × 150

Traipéisólach

80.0

AE -3

1000 × (115+135) × 130

Traipéisólach

46.0

AE -4

500 × (115+135) × 130

Traipéisólach

23.0

AE -5

1000 × (80+100) × 80

Traipéisólach

20.0

AE -6

500 × (105+135) × 100

Traipéisólach

16.0

AE -7

500 × (80+100) × 80

Traipéisólach

10.0

AE -8

400 × (110+120) × 50

Traipéisólach

7.0

AE -9

300 × (140+160) × 40

Traipéisólach

5.0

AE -10

200 × (90+110) × 40

Traipéisólach

3.0

AE -11

300 × 50

Diosca-chruthach

11.5

AE -12

360 × 40

Diosca-chruthach

9.0

AE -13

300 × 40

Diosca-chruthach

7.5

AE -14

200 × 50

Diosca-chruthach

4.0

AE -15

180 × 50

Diosca-chruthach

3.5

AE -16

120 × 100

Diosca-chruthach

2.5

industrial-interior-of-water-pump-valves-pressur-2025-03-18-19-21-31-utc

 

 

{5. Anóidí íobartach cóimhiotal alúmanaim a úsáidtear go coitianta le haghaidh cabhlacha loinge

Múnla

Toisí (A × B × C) / MM

Meáchan / kg

Ah -1

800×140×60

17.0

Ah -2

800×140×50

15.0

Ah -3

800×140×40

12.0

Ah -4

600×120×50

10.0

Ah -5

400×120×50

6.5

Ah -6

500×100×40

5.5

Ah -7

400×100×40

4.5

Ah -8

300×100×40

3.5

Ah -9

250×100×40

2.5

Ah -10

180×70×35

1.2

Ah -11

300×150×50

5.8

Ah -12

300×150×40

4.6

Ah -13

300×150×40

4.8

20250624172421

 

{6. Comhdhéanamh ceimiceach anóidí íobartach cóimhiotail alúmanaim

Cineál cóimhiotail

Comhdhéanamh Ceimiceach (%)

 

Zn

I gcaitheamh

Cfa

SNE

Mg

SI

Tí

Eisíontais (max)

AL (Iarmhéid)

               

SI

Fe

Cuir

 

---------------------------

-----

------

------

------

------

------

------

------

------

------

------

Al-Zn-in-CD

2.5-4.5

0.018-0.050

0.005-0.020

-

-

-

-

0.10

0.15

0.01

Forlíonadh

Al-Zn-in-SN

2.2-5.2

0.020-0.045

-

0.018-0.035

-

-

-

0.10

0.15

0.01

Forlíonadh

Al-Zn-in-Si

5.5-7.0

0.025-0.035

-

-

-

0.10-0.15

-

0.10

0.15

0.01

Forlíonadh

Al-Zn-in-SN-Mg

2.5-4.0

0.020-0.050

-

0.025-0.075

0.50-1.00

-

-

0.10

0.15

0.01

Forlíonadh

Al-Zn-in-mg-ti

4.0-7.0

0.020-0.050

-

-

0.50-1.50

-

0.01-0.08

0.10

0.15

0.01

Forlíonadh

{7. Feidhmíocht leictriceimiceach na n -anóidí íobartacha

Tíopáil

Poitéinseal Ciorcaid Oscailte (-V)

Poitéinseal Ciorcaid Dúnta (-V)

Toilleas iarbhír (a · h/kg)

Éifeachtúlacht reatha (%)

Iompar díscaoilte

AA-I

1.05-1.18

1.05-1.12

Níos mó ná nó cothrom le 2400

Níos mó ná nó cothrom le 85

Díscaoileadh aonfhoirmeach

AA-II

1.05-1.18

1.05-1.12

Níos mó ná nó cothrom le 2600

Níos mó ná nó cothrom le 92

Díscaoileadh aonfhoirmeach

20250624172513

 

Is féidir leis na hainmhithe alúmanaim a chuirimid ar fáil cosc a chur ar chreimeadh struchtúir cruach in uisce mara, agus úsáidtear iad go forleathan chun creimeadh a dhéanamh ar chabhail long, ar umair ballasta, ar phíblínte uisce mara, ar shaoráidí calafoirt agus duga, innealtóireacht amach ón gcósta, ardáin druileála, comhdhearcaithe, agus píblínte i gcomhdhéanamh na n -ithreach .} Tá feidhmíocht alumin ag cur i bhfeidhm ar an gcomhdháil difir an t -alloy. Comhdhéanamh chun riachtanais na gcustaiméirí a chomhlíonadh, agus is féidir linn anóidí a mhonarú le sonraíochtaí speisialta de réir riachtanais na gcustaiméirí .

 

 

{2. Anóid íobartach maignéisiam

 

 

20250625094854
 

The magnesium anode produced by our company adopts high quality raw materials to produce, the anode potential is negative, the electricity generated per unit mass is large, it is the ideal sacrificial anode material. It is suitable for cathodic protection of metal structures in soil, freshwater and seawater media, such as petroleum gas pipelines, storage tanks, hot water exchangers, condensers and so ar .

 

Déantar anóid íobartach cóimhiotal maignéisiam a tháirgeadh de réir an chaighdeáin náisiúnta GB/T 17731-2015 "Anóid íobartach cóimhiotal maignéisiam", agus tá an anóid a úsáidtear le haghaidh píblíne ag teacht le Sy/T 0019-97 "Cód Dearaidh do Chosaint Cathóidigh le haghaidh Cruach -Cruach As Cruach Adhlactha"

Iarr luachan

 

 

 

 

Sonraíochtaí Táirgí

 

 

20250624172432

Sonraíochtaí Comhdhéanamh Ceimiceach

Grád

Eilimintí cóimhiotalacha (%)

Eilimintí eisíontais (uasmhéid %)

Bal de

Zn

MN

Mg

Fe

Cuir

ní

SI

Caoiseach

----------

-----

-----

-----

-----

-----

-----

-----

-----

-----

MGAZ63B

5.3-6.7

2.5-3.5

0.15-0.60

Cothromaigh

0.003

0.01

0.001

0.08

-

MGAZ31B

2.5-3.5

0.60-1.4

0.20-1.0

Cothromaigh

0.003

0.01

0.001

0.08

0.04

MGMLC

Níos lú ná nó cothrom le 0.01

-

0.50-1.3

Cothromaigh

0.01

0.01

0.001

0.05

-

Mg

Níos lú ná nó cothrom le 0.02

Níos lú ná nó cothrom le 0.03

Níos lú ná nó cothrom le 0.01

Níos mó ná nó cothrom le 99.9%

0.005

0.004

0.001

0.01

-

Sonraíochtaí feidhmíochta leictriceimiceacha

Grád

Poitéinseal Ciorcaid Oscailte (V, Cu/Cuso₄)

Poitéinseal Ciorcaid Dúnta (V, Cu/Cuso₄)

Toilleas iarbhír (a · h/kg)

Éifeachtúlacht reatha (%)

MGAZ63B

1.57-1.67

1.52-1.57

Níos mó ná nó cothrom le 1210

Níos mó ná nó cothrom le 55

MGAZ31B

1.57-1.67

1.47-1.57

Níos mó ná nó cothrom le 1210

Níos mó ná nó cothrom le 55

Mgm1c

1.77-1.82

1.64-1.69

Níos mó ná nó cothrom le 1100

Níos mó ná nó cothrom le 50

7a5fbd697e41b2478ab0bfe3d050e77
20250624172507

Anóidí íobartacha maignéisiam aon phíosa

Múnla

Toisí (fad × (barr+bun) × airde) (mm)

Meáchan (kg)

Mg -22

700 × (130+150) × 125

22.00

Mg -14

700 × (120+100) × 102

14.00

Mg -11

700 × (110+90) × 88

11.00

Mg -8

700 × (95+75) × 75

8.00

Mg -4

350 × (95+75) × 75

4.00

Mg -2

350 × (55+60) × 55

2.00

Anóidí íobartacha le haghaidh umair degassing agus malartóirí teasa

Múnla

Toisí (mm)

Meáchan (kg)

Aschur reatha (MA)

Iarrchán

Me -1

500 × (105+135) × 100 (trapezoidal)

10.0

3471

Córais chéim gháis

Me -2

350 × (60+90) × 75 (trapezoidal)

4.0

2404

Córais chéim gháis

Me -3

φ200 × 50 (sorcóireach)

3.0

600

Malartóirí teasa

Me -4

200 × 140 × 50 (dronuilleogach)

2.0

1144

Malartóirí teasa

Me -5

φ100 × 80 (sorcóireach)

1.0

541

Malartóirí teasa

degassing tank

Tá na tréithe seo a leanas ag an táirge:

 

(1) domhantarraingt bheag shonrach agus poitéinseal diúltach;

 

(2) voltas tiomána ard go héifeachtúlacht iarainn agus íseal reatha; is

 

(3) atá oiriúnach go háirithe do mheán ard -fhriotaíocht . (le haghaidh friotachais níos mó ná

100Ω-M, moltar anóid íobartach maignéisiam stiall)

Réamhchúraimí le húsáid:

(1) Ba chóir tionchar le struchtúr cruach a sheachaint .

(2) Nuair a úsáidtear é san ithir, ba chóir é a adhlacadh in áit íseal agus fliuch .

(3) Nuair a úsáidtear é san ithir, ní mór an anóid a adhlacadh i mála filler .

.

.

 

{3. Anóid íobartach cóimhiotail since

20250625095344
 

Is féidir na hainmhithe since a sholáthraímid a úsáid chun cosaint chathóideacha struchtúr cruach a chosaint, mar shampla longa, áiseanna calafoirt, innealtóireacht mhuirí, píblínte miotail adhlactha, umair stórála, córais uisce fuaraithe sáile, etc . a chóimhiotal since a tháirgtear anóidí íobartacha de réir an chaighdeáin náisiúnta gb/t 4950-2002} {}} {}} {}} {1} {1} {}} {1} {1} {{\\ t Cloíonn anóid na bpíblínte agus na n -anóidí íobartacha le haghaidh píblínte cruach adhlactha {. freisin, cloíonn sé le Syito 019-97 "Cód Dearaidh do Chosaint anóid íobairt na bpíobáin chruach adhlactha" {}}}}}}}}}}}

Iarr luachan

 

Sonraíochtaí anóid ribín cóimhiotail since

 
Feidhmíocht táirge anóid stiall since

 

Úsáidtear stiall since den chuid is mó i logánú spáis caol (mar shampla píopa i gcásáil) agus ithir ard anodicity, uisce úr, chun umair ola nó struchtúir chruach eile a chosaint i leictrilít ard -anodicity .

 

★ Solúbthacht mhaith, éasca le suiteáil, éasca le héagsúlacht fad agus cruth anóid a dhéanamh, mar shampla bíseach, diosca;

★ Dáileadh reatha aonfhoirmeach, tá éifeachtúlacht reatha ard, níos mó ná 95%:

Is féidir mór a chur in oiriúint do ráta anodic leictreach níos airde den chomhshaol,

★ Ní gá soláthar cumhachta seachtrach a bheith agat, tá croí seoltaí leanúnach ag an stiall, naisc níos lú leictreacha

Is féidir ★ a thrasnú trí na hócáidí cúnga áitiúla agus na timpeallachtaí deacra, cur i bhfeidhm na ndaoine níos solúbtha,

★ Tá meáchan aonaid an domhain go dtí an leictreachas dearfach beag, an shen reatha mór:

★ Tá meáchan aonaid an domhain go dtí an leictreachas dearfach beag, agus is féidir an sruth leictreach a úsáid chun an umar ola nó an struchtúr cruach a chosaint . Shen Current:

★ Is féidir é a úsáid mar chuaille talún, scaoileadh AC, tintreach, cosaint trealaimh agus daoine

Tíopáil

Toisí (mm)

Aonadmheáchan

A (tiús)

B (leithead)

C (fad)

(g/cm)

Mór breise (a)

25.4

31.75

30.5

35.72

Mór (b)

15.88

22.23

61

17.82

Caighdeán (c)

12.7

14.29

152.5/305/1098

8.93

Beag (D)

8.73

11.91

305

3.72

 

20250625101142

 

How to install zinc ribbon anode in cathodic protection? - Knowledge -  Xi'an Howah Industry Technology Co.,Ltd

Comhdhéanamh ceimiceach anóidí íobartach ribín cóimhiotail since

 

Tíopáil

Al (%)

CD (%)

Fe (uas %)

PB (uasmhéid %)

Cu (uas %)

Zn (%)

Cineál I.

0.1-0.5

0.02-0.07

0.005

0.006

0.005

Cothromaigh

Cineál II

Níos lú ná nó cothrom le 0.005

Níos lú ná nó cothrom le 0.003

0.0014

0.003

0.002

Cothromaigh

Zn íonachta ard

Níos lú ná nó cothrom le 0.003

Níos lú ná nó cothrom le 0.002

0.001

0.003

0.001

Cothromaigh

 

Sonraíochtaí Táirgí

 
a11104d8a38a27aaf9115772ca18016

Comhdhéanamh ceimiceach anóidí íobartach cóimhiotail since

Eilimint cheimiceach

Bal de

Cfa

Eisíontais (uasmhéid %)

Ábhar (%)

0.3-0.6

0.05-0.12

Fe

Cuir

Pb

SI

Zn

0.005

0.005

0.006

0.125

Cothromaigh

Feidhmíocht leictriceimiceach anóidí íobartach cóimhiotail since

Táscaire feidhmíochta

Poitéinseal Ciorcaid Oscailte -V (SCE)

Poitéinseal Oibre -V (SCE)

Cumas iarbhír (A · H/kg)

Éifeachtúlacht reatha (%)

Iompar díscaoilte

I sáile

{-1.09 go -1.05

{-1.05 go -1.00

Níos mó ná nó cothrom le 780

Níos mó ná nó cothrom le 95

Táirgí creimthe dícheangail go héasca; díscaoileadh dromchla aonfhoirmeach

20250624172353
20250625112852

Sonraíochtaí anóidí íobartacha cabhail

Múnla

Toisí (A × B × C) mm

Cumraíocht

Meáchan (kg)

Zh -1

800×140×60

Caighdeánach

47.0

Zh -2

800×140×50

Caighdeánach

39.0

Zh -3

800×140×40

Caighdeánach

31.0

Zh -4

600×120×50

Caighdeánach

25.0

Zh -5

400×120×50

Caighdeánach

16.0

Zh -5

300×150×50

Cosa cruach dúbailte

14.5

Zh -6

500×100×40

Caighdeánach

13.6

Zh -6

300×150×40

Cosa cruach dúbailte

11.5

Zh -7

400×100×40

Caighdeánach

11.0

Zh -7

300×150×50

Bolgta

12.0

Zh -8

300×100×40

Caighdeánach

7.5

Zh -8

300×150×40

Bolgta

9.0

Zh -9

250×100×40

Caighdeánach

6.5

Zh -10

180×70×40

Caighdeánach

3.5

Anóidí caighdeánach íobartach le haghaidh umair uisce ballasta

Múnla

Toisí (a × (b 1+ b2) × c) mm mm

Meáchan (kg)

Zt -1

500 × (115+135) × 130

56.0

Zt -2

1500 × (65+75) × 70

50.0

Zt -3

500 × (110+130) × 120

50.0

Zt -4

1000 × (58.5+78.5) × 68

33.0

Zt -5

800 × (56+74) × 65

25.0

Zt -6

1150 × (48+54) × 51

20.0

Zt -7

250 × (80+100) × 85

13.0

Zt -8

200 × (70+90) × 70

7.5

20250625095457

 

 

photo-of-heavy-load-dockside-cranes-in-port-cargo-2025-02-02-20-27-03-utc

Anóidí íobartacha do struchtúir innealtóireachta calafoirt agus mara

Múnla

Toisí (a × (b 1+ b2) × c) mm mm

Meáchan (kg)

Zi -1

1000 × (115+135) × 130

115.0

Zi -2

750 × (115+135) × 130

85.0

Zi -3

500 × (115+135) × 130

56.0

Zi -4

500 × (105+135) × 100

40.0

Anóidí fada íobartacha stiall fhada do chórais fuaraithe uisce farraige

Múnla

Toisí (a × (b 1+ b2) × c) mm mm

Cruth

Meáchan (kg)

Ze -1

500 × (115+135) × 130

Traipéisólach

56.0

Ze -2

1000 × (80+100) × 80

Traipéisólach

50.0

Ze -3

500 × (105+135) × 100

Traipéisólach

40.0

Ze -4

500 × (80+100) × 80

Traipéisólach

25.0

Ze -5

400 × (110+120) × 50

Traipéisólach

16.0

Ze -6

300 × (140+160) × 40

Traipéisólach

12.5

Ze -7

200 × (90+110) × 40

Traipéisólach

5.5

Ze -8

300 × 60

Cíosa

30.0

Ze -9

360 × 40

Cíosa

28.5

Ze -10

300 × 40

Cíosa

20.0

Ze -11

200 × 50

Cíosa

10.5

Ze -12

180 × 50

Cíosa

8.5

Ze -13

120 × 100

Cíosa

7.5

inside-view-of-pipe-lines-in-a-factory-2025-02-09-01-12-06-utc 1
storage tank

Anóidí íobartacha le haghaidh cosaint creimthe inmheánach umar

Múnla

Toisí (a × (b 1+ b2) × c) mm mm

Meáchan (kg)

Zc -1

750 × (115+135) × 130

85.0

Zc -2

500 × (115+135) × 130

56.0

Zc -3

500 × (105+135) × 100

40.0

Zc -4

300 × (105+135) × 100

25.0

Anóidí íobartacha le haghaidh píblínte adhlactha

Múnla

Toisí (a × (b 1+ b2) × c) mm mm

Meáchan (kg)

Zp -1

1000 × (78+88) × 85

50.0

Zp -2

1000 × (65+75) × 65

33.0

Zp -3

800 × (60+80) × 65

25.0

Zp -4

800 × (55+64) × 60

22.0

Zp -5

650 × (58+64) × 60

18.0

Zp -6

550 × (58+64) × 60

15.0

Zp -7

600 × (52+56) × 54

12.5

Zp -8

600 × (40+48) × 45

9.0

buried pip

 

 

 Cliceáil ar an liosta táirgí thíos le haghaidh tuilleadh sonraí táirge

Cosaint anóid íobartach catóidigh

 

20250625111431

Is é an modh cosanta catóide íobartach, ar a dtugtar modh cosanta anóid íobartach, mar cheann den dá chineál cosanta catóide, an modh cosanta is luaithe de theicneolaíocht chosanta leictriceimiceach . An modh cosanta a bhaineann le creimeadh miotail a chosc, is é sin an miotal athfhriotail a úsáid mar mhiotal athfhriotail, agus an miotal cosanta a bhaineann le miotal a cheangal chun a fhoirmiú chun an t -imoibriú miotail agus an t -ocsaídiú miotail a cheangal chun a fhoirmiú chun a fhoirmiú chun an t -imoibriú agus an miotal a cheangal le chéile chun an t -imoibriú a cheangal chun an t -ocsaídiú a cheangal chun an t -imoibriú a cheangal chun an t -imoibriú a cheangal chun a fhoirmiú chun an t -imoibriú a cheangal chun an t -imoibriú agus an miotal a cheangal chun an t -imoibriú agus an miotal a cheangal chun an t -imoibriú agus an miotal a cheangal chun an t -imoibriú. Tomhaltas, is féidir an miotal cosanta mar leictreoid dhearfach a sheachaint creimeadh .

Is minic a úsáidtear modh cosanta catóide anóid íobartach chun cosanta a dhéanamh ar chairn cruach san uisce, sliogáin línéar aigéin, srl

 

Sainmhíniú:
 

Príomhúil

Sainmhíniú 1: Déantar an anóid a chaitear de réir a chéile leis an sruth atá ag dul as oifig, mar sin tugtar anóid íobartach air, ídítear an anóid seo go tapa, ní mór go mbeadh an suíomh agus an modh suiteála éasca a chur in ionad . Ábhair mhiotail íseal-phoitéinseal san áireamh maignéisiam, cóimhiotal maignéisiam, pure zinc, zinc alloy, aluminum alloy agus mar sin ar {}}}}}}}}}}}} {}, {}, a:::

 

Sainmhíniú 2: Tugtar modh anóid íobartach ar an modh seo ar chosaint chathóidigh ar mhiotail ghníomhacha nó ar chóimhiotail ghníomhacha den sórt sin anóid íobartach . Anóid íobartach cosanta catóide an cur i bhfeidhm is luaithe ar theicneolaíocht cosanta leictriceimiceach .

 

Sainmhíniú 3: Chun cosaint an anóid a fháil, ídítear an anóid de réir a chéile, mar sin tugtar anóid íobartach air . Is é an modh reatha éigeantach sruth catóide a chur i bhfeidhm ar an struchtúr miotail cosanta agus ar shruth anodic ar an anóid chúnta, arb ionann é agus creimeadh faoi láthair, ionas go gcosnaítear an struchtúr miotail .}}}

 

700578600b156ba0608678e7c2179f5

 

Idirmheánach

Sainmhíniú 4: Ós rud é go soláthraíonn creimeadh na miotail seo cosaint don bhunchill creimthe agus go luathaíonn a chreimeadh féin, tugtar anóid íobartach air . Ba chóir go mbeadh an t -ábhar anóid íobartach in ann na riachtanais seo a leanas a chomhlíonadh: (l) Ba chóir go mbeadh poitéinseal diúltach leordhóthanach aige agus go mbeadh sé cobhsaí .

 

Sainmhíniú 5: Modh anóid íobartach (: sacrificialanode) déanta as ábhair mhiotail le poitéinseal diúltach, nuair a bhíonn sé ceangailte leis an bpíblíne faoi chosaint, tarlaíonn a dhí -chomhcheangal tosaíochta féin, rud a chuireann cosc ar chreimeadh na píblíne, mar sin tugtar anóid íobartach air an t -am céanna a bhfuil an t -am céanna ag an am céanna ag an am céanna ag an am céanna ag an am a bhfuil an t -am ag an am céanna ag an am a bhfuil an t -am céanna ag an gcosaint a bhfuil an t -am céanna ag an gcosaint ag an am céanna. Leictreachas teoiriciúil, ach freisin éifeachtúlacht reatha ard agus chobhsaí .

 

Sainmhíniú 6: Tugtar anóid íobartach {. ar mhiotal nó cóimhiotal a bhfuil poitéinseal neodrach diúltach go leor ann . ag cur san áireamh an gás amhola féin contúirt phléascach chun sruthanna fáin a sheachaint, níl umair stórála amhola taobh istigh d'úsáid an mhodha um chosc creimthe reatha iontaofa .

 

Sainmhíniú 7: Sa chatóid (struchtúr cosanta) atá le cosaint ag an am céanna, ídítear an t -anóid i gcónaí, mar sin tugtar an anóid íobartach air . 3 ábhar anóid idéalach Is é maignéisiam, alúmanam agus since, tá siad i dtimpeallacht nádúrtha an chreimthe thíos {{}} v} v (athbheochan, CUSO4} {{{}}}}}}} {} {} {}} {}}}}}}}}} 9}}}}}}}}}}} RENTE} ag sroicheadh an sroicheann}:}}}}}}}}}}}} {}} {}}}}}}} {}

Chun cinn

Sainmhíniú 8: Tugtar anóidí íobartach ar leictreoidí a bhfuil poitéinseal diúltach acu mar go gcaitear an t -ábhar anóid de réir mar a leanann an sruth ag sreabhadh . mar ábhar anóid íobartach, ní mór do mhiotal nó cóimhiotal na coinníollacha seo a leanas a chomhlíonadh [1]: (1) Tá an poitéinseal diúltach go leor chun leictreoin leordhóthanacha a sholáthar chun an trealamh miotail cosanta a dhéanamh pololization catodic {{{}}}}

 

 

Bheith

 

20250625112852

 

baiduimg.webp

Buntáistí

1. Níl aon soláthar cumhachta seachtrach ag teastáil;

{2. Is beag cothabháil;

{3. Is é an toradh a bhíonn ar aschur beag reatha ná beagán cur isteach reatha nó gan aon fhásach;

4. éasca a shuiteáil;

{5. éasca anóid a chur leis i bhformhór na gcásanna;

Soláthraíonn 6. dáileadh reatha aonfhoirmeach;

baiduimg.webp

Míbhuntáistí

{1. Voltas tiomána níos ísle/sruth;

Éilíonn 2. níos mó anóidí le haghaidh struchtúir atá brataithe go dona;

D'fhéadfadh 3. a bheith neamhéifeachtach i dtimpeallachtaí ithreach friotaíochta ard;

{4. Costas níos airde in aghaidh an ampere reatha ná an chosaint chathóidigh reatha mar gheall ar éifeachtúlacht reatha níos ísle (tomhaltas féin-creimthe);

{5. Tá sé deacair nó costasach athsholáthar a dhéanamh ar anóidí caite .

 

Riachtanais an Chórais

 

20250624172447

 

De ghnáth ní úsáidtear anóidí íobartacha ach go heacnamaíoch ar struchtúir le riachtanais reatha cosanta íseal agus i dtimpeallachtaí friotachais ithreach íseal . Ina theannta sin, níl iontu ach luach nuair nach bhfuil coinníollacha soláthair cumhachta ar fáil nó nuair a thagann cásanna neamh -eacnamaíocha chun cinn .

 

Sacrificial anode materials suitable for use in soil are mainly magnesium, and in seawater zinc and aluminum. In order to keep the current output as stable as possible and to reduce the anode grounding resistance, the sacrificial anode in soil should be surrounded by a chemical filler consisting mainly of a mixture of 75% calcium sulfate, 20% bentonite and 5% sodium Sulfate {. Níor chóir anóidí íobartacha a chur i gcóc, agus nuair a úsáidtear iad i ngrúpaí, ba cheart go mbeadh an spásáil anóid 3 m . ar a laghad tiús an chlúdaigh ithreach ar bharr na n -anóid Ar an bpíblíne trí bhosca tomhais, agus níor chóir go mbeadh an voltas marthanach AC ar chorp an anóid níos mó ná 20 V nuair a úsáidtear an anóid íobartach i gcomharsanacht chóras tarraingthe AC.

 

 

Riachtanais Anóid

 

1, tá an poitéinseal diúltach go leor, ach níl sé ró -dhiúltach, ionas nach dtáirgeann sé imoibriú deasctha hidrigine sa limistéar catóide;

 

2, ba chóir go mbeadh ráta polaraithe an anóid beag, agus ba chóir go mbeadh an t -aschur reatha cuaille potentiodynamic cobhsaí;

 

3, ba chóir go mbeadh toilleas an ábhair anóid mhór;

 

4, ní mór éifeachtúlacht ard reatha a bheith ann;

 

5, díscaoileadh an t -aonchineálach . a dhíscaoileadh go héasca;

 

6, tá an t -ábhar saor agus foinsithe go leordhóthanach .

 

7, ba chóir go mbeadh na táirgí creimthe mar thoradh air neamhthocsaineach agus neamhdhíobhálach, gan aon truailliú ar an gcomhshaol, gan aon chontúirt a bhaineann le sláinte an phobail;

20250624172455

Tógáil agus suiteáil

 

a85c7eb1d45e8d1bd3263e389c28e37

{1. Déanfar anóidí íobartacha bagged a chur ar ais le hábhar atá comhbhrúite go cuí . Nuair a sholáthraítear anóid ar leithligh ón ábhar pacála speisialta, cuirfear an anóid i lár an ábhair phacála agus déanfar an t -ábhar pacála a dhíriú ar gach duine a chinntítear go n -áireofaí agus go gcinnteofar go n -áireofaí na hoibrithe go léir go n -áireofaí go n -oibreodh na hOlltóirí go léir go n -áireofaí go n -oibreodh na hOllmhúcháin agus go n -oibreodh na hOlltóirí go n -iompraíonn siad go n -iompraíonn na hOibreacha go léir go n -oibreodh na hOibreacha go n -iompraíonn na hOlltóirí damáiste . Chun strus teanntachta a sheachaint, ba chóir an seoltóir a fhágáil le dóthain duillín .

2. Where bracelet-type anodes are used, the pipe cover beneath the anode shall be free of defects. Installation of bracelet anodes should be done carefully to prevent damage to the cover. If concrete is sprayed on the pipe, all concrete should be removed from the surface of the anode. If reinforced Úsáidtear coincréit, tá toirmeasc ar theagmháil miotail idir an anóid agus an mogalra athneartaithe nó idir an mogalra athneartaithe agus an píopa .

{3. Nuair a úsáidtear anóidí bagged, is féidir iad a adhlacadh trí thrinse a thochailt nó trí fhill a threabhadh, le líontóir ceimiceach nó gan é de réir mar is gá, de ghnáth comhthreomhar leis an gcuid píopa den phíobán á chosaint .

 

 

 

Iarratais Táirgí

 

rnli-lifeboat-scarborough-england-2025-03-18-14-51-29-utc
heat exchanger
buried pip
1

Comhlaí ar phíblínte adhlactha le cosaint an -lag nó gan aon chreimeadh ar chor ar bith;

 
2

Réimsí ina ndearnadh damáiste mór do chásáil nó clúdaigh ghearra;

 
3

Limistéir ina dtarlaíonn sciath leictreach, ar chóir dó an sruth éifeachtach a mhaolú ó chóras reatha feidhmithe i bhfad i gcéin;

 
4

Má tharlaíonn cur isteach anodic faoi chúinsí oiriúnacha, is féidir anóidí íobartacha a úsáid ag pointe draein na píblíne chun an sruth atá ag cur isteach ar an bpíblíne a chur ar ais go dtí foinse na srutha cur isteach .

 
5

I gcás ceantair ina bhfuil go leor struchtúr agus castacht adhlactha, tá sé an -deacair cosaint chathóidigh reatha a chur i bhfeidhm gan cur isteach ar struchtúir atá gar do chóngaracht . do struchtúir sa timpeallacht seo, is é an modh anóid íobartach an rogha níos eacnamaíche .

 
6

Úsáidtear anóidí íobartach go forleathan chun ballaí istigh na malartóirí agus na soithí eile .

 
7

Maidir le struchtúir mhara domhain, is féidir anóidí íobartacha móra a úsáid chun comhpháirteanna faoi uisce a chosaint .

 
8

Déantar méid áirithe bloic since a luchtú ar shtern loinge agus ar an gcuid de chabhail na loinge faoi bhun na líne uisce chun creimeadh chabhail na loinge a chosc, srl .

 

 

Airíonna faoi uisce

 

20250624172949

Úsáidtear anóidí íobartacha le haghaidh struchtúir mhiotail faoi uisce, agus de ghnáth déantar tomhais uair amháin gach 3 mhí nó mar sin, go príomha chun poitéinseal gach pointe tomhais a thomhas, luachanna aschuir anóid agus luachanna eile .

 

Ba chóir a thabhairt faoi deara freisin go bhfuil cáblaí ceangailte leis an anóid le miotal an struchtúir faoi uisce, agus ba chóir na cáblaí a iniúchadh go rialta chun deisiú tráthúil damáiste a sheachaint de bharr tonnta agus longa .

 

Nuair nach bhfuil poitéinseal cosanta an struchtúir go huisce diúltach go leor, is gá an anóid a athsholáthar, ach smaoinigh ar anóid eile a mholadh le haghaidh cigireachta .

 

Tá an anóid íobartach socraithe sa struchtúr faoi uisce, nach féidir leis an sruth aschuir a thomhas, ach amháin de réir an tomhais fhéideartha chosanta .

 

Uaireanta bíonn tionchar ag an méid truaillithe ar uisce mara ar fheidhmíocht oibre anóid .

 

 

Onóir agus cáilíocht
 
 

Deimhniú Oifigiúil, Seirbhís Gairmiúil Iar -Díolacháin .

Honor1
 
Honor8
 
Honor6
 
Honor6
 
Honor7
 

 

 

Trealamh próiseála

1

Trealamh leá

2

Trealamh a Chruthú

3

Líne táirgthe picilte

4

Trealamh rollach pláta

5

Trealamh Stampála

6

Trealamh Cóireála Dromchla

7

Ionad meaisínithe

8

Saotharlann cheimice

 

 

Próiseas braite

1

Tástáil tríthoiseach

2

Tástáil Méid Gráin

3

Tástáil teanntachta pláta

4

Locht a bhrath

5

Meaisín tomhais optúil trí chomhordú

6

Cmm

7

Anóid ag neartú Tástáil saoil

8

Tástáil Comhdhéanamh Anóid

productcate-1204-545

 

Déan teagmháil linn

 

 
Táimid anseo duitse

 

Ag tabhairt cuairte orainn
Seoladh: Níl . 28, Páirc Tionscail Gaoya, Ceantar Gaoxin, Cathair Baoji, Cúige Shaanxi .
Facs
Uimhir: 0086-0917-3292780
Déan teagmháil dhíreach
Fón:

{+86 15619363855 Edward wu
{+86 18700703333 elsa lin

+86 15291791403

Eve Zhang

 

Iarr luachan

 

 